MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® ECO 4056B TPC Polyester Elastomer
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D High Performance Polyester Elastomer certified bio-circular according to ISCC Plus mass balance approach

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Melt Density 1.02 g/cc0.0368 lb/in³
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
Sim. to ISO 62
 0.70 %
@Thickness 2.00 mm
0.70 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Water Vapor Transmission 450 g/m²/day
@Thickness 0.0250 mm
29.0 g/100 in²/day
@Thickness 0.000984 in
DIS 15106-1/-2
Oxygen Transmission 350 cc-mm/m²-24hr-atm
@Thickness 0.0250 mm
889 cc-mil/100 in²-24hr-atm
@Thickness 0.000984 in
23°C/85%r.h.; DIS 15105-1/-2
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/inISO 294-4, 2577
Melt Flow 5.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.6 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Puncture Resistance  1500 N
@Temperature 23.0 °C
337 lb (f)
@Temperature 73.4 °F
Puncture - maximum force; ISO 6603-2
 2800 N
@Temperature -30.0 °C
629 lb (f)
@Temperature -22.0 °F
Puncture - maximum force; ISO 6603-2
Hardness, Shore D 3737ISO 48-4 / ISO 868
 4343ISO 868
Tensile Strength, Yield  2.40 MPa
@Strain 5.0 %
348 psi
@Strain 5.0 %
ISO 527-1/-2
 4.60 MPa
@Strain 10 %
667 psi
@Strain 10 %
ISO 527-1/-2
Tensile Modulus 0.0600 GPa8.70 ksiISO 527-1/-2
50% Modulus 8.40 MPa
@Strain 50 %
8.40 MPa
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 0.0600 GPa8.70 ksiISO 178
Poissons Ratio 0.500.50
Izod Impact, Notched (ISO)  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eA
Tensile Impact Strength 230 kJ/m²
@Temperature 23.0 °C
109 ft-lb/in²
@Temperature 73.4 °F
Notched; ISO 8256/1
Puncture Energy  19.0 J
@Temperature 23.0 °C
14.0 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 37.0 J
@Temperature -30.0 °C
27.3 ft-lb
@Temperature -22.0 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 54.0 MPa7830 psiISO 899-1
Tensile Creep Modulus, 1000 hours 40.0 MPa5800 psiISO 899-1
Tear Strength 96.0 kN/m548 plinormal; ISO 34-1
 102 kN/m582 pliparallel; ISO 34-1
Abrasion 200200mm³; ISO 4649
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.00e+10 ohm-cm7.00e+10 ohm-cmIEC 62631-3-1
Surface Resistance 2.00e+14 ohm2.00e+14 ohmIEC 62631-3-2
Dielectric Constant  4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 62631-2-1
 5.2
@Frequency 100 Hz
5.2
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 18.0 kV/mm457 kV/inIEC 60243-1
Dissipation Factor  0.011
@Frequency 100 Hz
0.011
@Frequency 100 Hz
IEC 62631-2-1
 0.0525
@Frequency 1e+6 Hz
0.0525
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 130 µm/m-°C72.2 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 160 µm/m-°C88.9 µin/in-°FISO 11359-1/-2
Melting Point 152 °C306 °F10°C/min; ISO 11357-1/-3
Brittleness Temperature -97.0 °C-143 °FISO 974
Glass Transition Temp, Tg -50.0 °C-58.0 °F10°C/min; ISO 11357-1/-3
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
 HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
IEC 60695-11-10
Oxygen Index 20 %20 %ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 170 °C338 °FOptimum
 165 - 180 °C329 - 356 °F
 170 - 190 °C338 - 374 °F
 180 °C356 °FOptimum
Mold Temperature 30.0 - 40.0 °C86.0 - 104 °F
 40.0 °C104 °FOptimum
Drying Temperature 80.0 °C176 °F
 70.0 - 90.0 °C158 - 194 °F
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer
 2.00 - 3.00 hour2.00 - 3.00 hourDehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %
 <= 0.080 %<= 0.080 %
 
Descriptive Properties
AdditivesBiobased
Drying Recommended?yes
Eff. thermal diffusivity (m²/s)8.50E-08
FMVSS ClassSEISO 3795 (FMVSS 302)
PolymerTPC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX5195e / 295968

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.