System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ THERMOTUF™ Compound VF1001S Polyamide, Unspecified (Nylon, Unspecified)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
Material Notes:
LNP THERMOTUF VF1001S compound is based on Super Tough Nylon resin containing 5% glass fiber. Added features of this grade include: Heat Stabilized, Impact Modified.
Features: Impact Modified,Heat Stabilized
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.12
g/cc
0.0405
lb/in³
ASTM D792
1.12
g/cc
0.0405
lb/in³
ISO 1183
Moisture Absorption
0.150 - 0.250 %
0.150 - 0.250 %
Injection Molding
0.680 %
0.680 %
23°C/50% RH/24 hrs; ASTM D570
1.10 %
1.10 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.010
-
0.030
cm/cm
0.010
-
0.030
in/in
24hrs; ASTM D955
Linear Mold Shrinkage, Transverse
0.010
-
0.030
cm/cm
0.010
-
0.030
in/in
24hrs; ASTM D955
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
56.0
MPa
8120
psi
5 mm/min; ASTM D638
56.0
MPa
8120
psi
5 mm/min; ISO 527
Tensile Strength, Yield
61.0
MPa
8850
psi
5 mm/min; ASTM D638
61.0
MPa
8850
psi
5 mm/min; ISO 527
Elongation at Break
7.6 %
7.6 %
5 mm/min; ISO 527
9.3 %
9.3 %
5 mm/min; ASTM D638
Elongation at Yield
3.4 %
3.4 %
5 mm/min; ASTM D638
3.4 %
3.4 %
5 mm/min; ISO 527
Tensile Modulus
3.29
GPa
477
ksi
1 mm/min; ISO 527
3.39
GPa
492
ksi
5 mm/min; ASTM D638
Flexural Strength
86.0
MPa
12500
psi
ISO 178
Flexural Modulus
2.76
GPa
400
ksi
2 mm/min; ISO 178
2.94
GPa
426
ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
106
J
78.2
ft-lb
ASTM D256
Izod Impact, Unnotched
7.20
J/cm
13.5
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
9.00
kJ/m²
4.28
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
41.0
kJ/m²
19.5
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
8.00
J
5.90
ft-lb
ASTM D3763
Impact Test
11.0
J
8.11
ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
64.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
35.6
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
CTE, linear, Transverse to Flow
98.0
µm/m-°C
@Temperature -30.0 - 30.0 °C
54.4
µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi)
242
°C
468
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
249
°C
@Thickness 3.20 mm
480
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
154
°C
309
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
198
°C
@Thickness 3.20 mm
388
°F
@Thickness 0.126 in
unannealed; ASTM D648
Processing Properties
Metric
English
Comments
Zone 2
270
-
280
°C
518
-
536
°F
Zone 3
290
-
300
°C
554
-
572
°F
Melt Temperature
270
-
295
°C
518
-
563
°F
Injection Molding
Mold Temperature
50.0
-
95.0
°C
122
-
203
°F
Drying Temperature
80.0
°C
176
°F
Injection Molding
Dry Time
4.00
hour
4.00
hour
Injection Molding
Back Pressure
0.300
-
0.700
MPa
43.5
-
102
psi
Screw Speed
10
-
60
rpm
10
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH82029 / 289976
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.