MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Protective Coating PC-Xtreme™ Crack and Joint Filler
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: PC-Xtreme™ is a two-component (1:1 ratio), rapid curing Polyurea elastomeric crack and joint filler. It is self leveling, 100% solids with Extreme flexibility allowing 10-15% movement of installed joint width. Non solvent formula with low V.O.C. (0 g/l).

Data provided by Protective Coating Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 525 cP525 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8075 - 80ASTM D2240
Elongation at Break 82 %82 %ASTM D412
Adhesive Bond Strength 2.76 MPa400 psiLap Shear Tensile; ASTM C882
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 3.00e+10 ohm3.00e+10 ohmASTM D257
Dielectric Strength 11.8 kV/mm300 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 48.9 °C120 °F
Shrinkage <= 1.0 %<= 1.0 %ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  720 min
@Temperature 49.0 °C
12.0 hour
@Temperature 120 °F
 1440 min
@Temperature 24.0 °C
24.0 hour
@Temperature 75.2 °F
Service Time; ASTM D1002
 2880 min
@Temperature -24.0 °C
48.0 hour
@Temperature -11.2 °F
Full Cure
Working Life 150 min
@Temperature 23.9 °C
150 min
@Temperature 75.0 °F
 
Descriptive Properties
ColorMetallic GrayMixed
Form2 Part PasteWet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEPXP98 / 280635

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.