LNP LUBRICOMP DL002ER compound is based on Polycarbonate (PC) resin containing 10% PTFE. Added features of this grade include: Wear Resistant, Easy Molding, Mold Release. Features: Wear resistant,Good Moldability,Good Mold Release,Easy Molding Information provided by SABIC |