MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultramid® STAR S 218 V30 BLACK 31N Nylon 6, 30% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled; Nylon 6, Heat Stabilized

Material Notes: Product Description: Ultramid® STAR S 218 V30 BLACK 31N is based on a patented high flow polyamide 6 resin, heat stabilized, reinforced with 30% of glass fiber, for injection molding. Due to its outstanding flow characteristics, this grade provides a significant productivity improvement and allows more freedom in mold and part design versus a standard polyamide solutions.

Availability: Africa & Middle East; Asia Pacific; North America

Filler/Reinforcement: Glass Fiber, 30% Filler by Weight

Additive: Heat Stabilizer

Features: Good Dimensional Stability; Good Mold Release; Heat Stabilized – Inorganic; High Flow; Outstanding Surface Finish

Uses: Consumer Applications; Furniture; General Purpose; Industrial Applications

Agency Ratings: EC 1907/2006 (REACH); EU 2011/65/EC; EU 2015/863 RoHS3

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA6-GF30

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Water Absorption 2.0 %Equilibrium, 50% RH; ISO 62
 0.95 %
@Time 86400 sec
ISO 62
Maximum Moisture Content 0.20
Linear Mold Shrinkage, Flow 0.0080 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0015 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23800 psiASTM D638
 26100 psiISO 527-2
Elongation at Break 3.0 %ASTM D638
 3.0 %ISO 527-2
Tensile Modulus 1.45e+6 psiISO 527-1
Flexural Strength 34800 psiASTM D790
Flexural Modulus 1.31e+6 psiISO 178
 1.33e+6 psiASTM D790
Izod Impact, Notched (ISO) 2.10 ft-lb/in²ASTM D256
 5.20 ft-lb/in²
@Temperature 22.8 °C
ISO 180/A
 5.70 ft-lb/in²
@Temperature -30.0 °C
ISO 180/A
Izod Impact, Unnotched (ISO) 32.0 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 17.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 31.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 3.30 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 4.80 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 432 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 401 °FUnannealed; ASTM D648
 401 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 3.30 mm
IEC 60695-11-10,-20
Glow Wire Flammability Index 1200 °F
@Thickness 1.52 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 446 - 455 °F
Middle Barrel Temperature 455 - 464 °F
Front Barrel Temperature 464 - 473 °F
Mold Temperature 140 - 194 °F
Drying Temperature 176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASG2044 / 310737

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.