LNP ELCRIN WF006XiQ compound is based on Polybutylene terephthalate (PBT) resin utilizing ELCRIN iQ upcycling technology containing minimum 37% Post-Consumer Recycling (PCR) weight content and 30% glass fiber. Added features of this grade include: Excellent Strength, Stiffness and Dimensional Stability. Potential applications may include handles, connectors. Features: Post-Consumer Recycled (PCR) content,High Stiffness,High Strength,Good dimensional stability Information provided by SABIC |