MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRILOY™ Compound K2000 Acetal (POM) Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRILOY K2000 compound is based on Acetal (POM) resin containing proprietary lubricant. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccASTM D792
 1.40 g/ccISO 1183
Moisture Absorption 0.330 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.022 cm/cm24hrs; ASTM D955
 0.0221 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0214 cm/cm24hrs; ISO 294
 0.023 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 51.0 MPaASTM D638
 59.0 MPaISO 527
Tensile Strength, Yield 55.0 MPaASTM D638
 60.0 MPaISO 527
Elongation at Break 13.3 %ISO 527
 32.4 %ASTM D638
Elongation at Yield 9.0 %ISO 527
 9.3 %ASTM D638
Tensile Modulus 2060 MPa50 mm/min; ASTM D638
 2560 MPa1 mm/min; ISO 527
Flexural Strength 65.0 MPaISO 178
 84.0 MPaASTM D790
Flexural Modulus 2420 MPaASTM D790
 2420 MPaISO 178
Izod Impact Notched 69.0 JASTM D256
Izod Impact, Unnotched 1356 J/mASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 48.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 Jpeak; ASTM D3763
Coefficient of Friction, Dynamic 0.38ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.24ASTM D3702 Modified: Manual
K (wear) Factor 10.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 115 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 115 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 111 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 111 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 110 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 195 - 205 °C
Zone 3 210 - 220 °C
Melt Temperature 200 - 215 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81139 / 289086

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.