MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL GTX™ Resin GTX951A Polyphenylene Ether + PA (PPE+Nylon)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX951A resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, high melt flow, and added mold release. NORYL GTX951W resin was designed for automotive under-the-hood applications such as power distribution boxes, relay boxes, and junction boxes.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Good Processability,Good Moldability,Good Mold Release

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Water Absorption 1.99 %
@Time 86400 sec
1.99 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Moisture Absorption at Equilibrium 0.39 %0.39 %23°C/50% RH; ISO 62-4
Linear Mold Shrinkage, Flow 0.014 - 0.017 cm/cm0.014 - 0.017 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.015 cm/cm0.012 - 0.015 in/in24hrs; ASTM D955
Melt Flow  24 g/10 min
@Load 2.16 kg,
Temperature 280 °C
24 g/10 min
@Load 4.76 lb,
Temperature 536 °F
ASTM D1238
 65 g/10 min
@Load 5.00 kg,
Temperature 280 °C
65 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 57.0 MPa8270 psi50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa9430 psi50 mm/min; ASTM D638
 66.0 MPa9570 psi50 mm/min; ISO 527
Elongation at Break 51 %51 %50 mm/min; ISO 527
 55 %55 %50 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.25 GPa326 ksi50 mm/min; ASTM D638
Flexural Strength 98.0 MPa14200 psibreak, 2mm/min; ISO 178
 100 MPa14500 psibrk, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2.37 GPa344 ksi2 mm/min; ISO 178
 2.55 GPa370 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 211 J156 ft-lbASTM D256
 100 J
@Temperature -30.0 °C
73.8 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²63.5*12.7*3.2, 23°C; ISO 180/4A
 8.00 kJ/m²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
63.5*12.7*3.2, 23°C; ISO 180/4A
Charpy Impact, Notched 2.10 J/cm²9.99 ft-lb/in²ISO 179/2C
 1.00 J/cm²
@Temperature -20.0 °C
4.76 ft-lb/in²
@Temperature -4.00 °F
ISO 179/2C
Dart Drop, Total Energy 48.0 J35.4 ft-lbpeak; ASTM D3763
 32.0 J
@Temperature -30.0 °C
23.6 ft-lb
@Temperature -22.0 °F
peak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 22.4 kV/mm
@Thickness 1.60 mm
569 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
Dissipation Factor 0.017
@Frequency 1e+6 Hz
0.017
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 167 µm/m-°C
@Temperature 60.0 - 138 °C
92.8 µin/in-°F
@Temperature 140 - 280 °F
ASTM E831
CTE, linear, Transverse to Flow  85.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
47.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 153 µm/m-°C
@Temperature 60.0 - 138 °C
85.0 µin/in-°F
@Temperature 140 - 280 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 181 °C358 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 195 °C
@Thickness 6.40 mm
383 °F
@Thickness 0.252 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 270 - 295 °C518 - 563 °F
Zone 2 260 - 295 °C500 - 563 °F
Zone 3 265 - 295 °C509 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °FInjection Molding
Mold Temperature 65.0 - 95.0 °C149 - 203 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82179 / 290126

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.