MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEMUV-709 Highly Effective Anti- UV/Anti-Yellowing Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: GOYENCHEMUV-709 is particularly suitable for agricultural films as it exhibits great anti-sulfide performance. With low volatility, no migration, and excellent high polymer compatibility which provides great processibility to polymers, GOYENCHEMUV-709 can be used in polyolefin, olefin copolymer, polyacetals, polyamides, polyurethane, etc., and now has been an appointed product to numerous film manufacturers.

Advantages:

  • Provides polymers with outstanding anti-UV and anti yellowing effect
  • Provides polymers with long-term heat stability
  • Particularly suitable for agricultural films as it exhibits great anti-sulfide performance
  • Suitable for use during polymerization or post adding (compound)
  • Low volatility
  • No migration
  • Effectively prevents physical properties change of polymer caused by oxygen or other environmental factors
Applications:
  • Polyolefin: PP, PE, HDPE, LDPE, LLDPE
  • Olefin copolymer: EVA
  • Polyurethane: PU resin, PU coating, PU coating finish, etc.
  • TPU: TPU resin, TPU elastomer, TPU adhesive, TPU hot glue, etc.
  • Polyamides
  • Polyacetals
  • Tackifier resins
  • TPU injection or extrusion molding
  • Soft/Hard PVC, PVC blend
  • Thermoplastics
  • Thermoplastic resins

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AppearancePowder
ColorLight yellow
Purity100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN488 / 266796

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.