MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ RFD02 PA 66 (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LNP STAT-KON RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccASTM D 792
 1.30 g/ccISO 1183
Moisture Absorption 0.500 %
@Time 86400 sec
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
@Time 86400 sec
ASTM D 955
 0.011 cm/cm
@Time 86400 sec
ISO 294
Linear Mold Shrinkage, Transverse 0.015 cm/cm
@Time 86400 sec
ISO 294
 0.014 - 0.016 cm/cm
@Time 86400 sec
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 74.0 MPaISO 527
 77.0 MPaASTM D 638
Elongation at Break 5.1 %ISO 527
 5.5 %ASTM D 638
Tensile Modulus 7400 MPa1 mm/min; ISO 527
 8270 MPa50 mm/min; ASTM D 638
Flexural Strength 131 MPaASTM D 790
 139 MPaISO 178
Flexural Modulus 5510 MPaASTM D 790
 6300 MPaISO 178
Izod Impact, Notched 37.0 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 213 J/m
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 3.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 14.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 ohm - 1e+05ASTM D 257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 69.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 46.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 48.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 256 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 252 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 239 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 236 °C
@Thickness 3.20 mm
unannealed; ASTM D 648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber

PSABI48186 / 189271

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.