MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound DP003 Polycarbonate (PC) (Americas)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP LUBRICOMP DP003 compound is based on Polycarbonate (PC) resin containing 15% PTFE/silicone. Added features of this grade include: Wear Resistant.

Features: Wear resistant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.26 g/ccASTM D792
 1.26 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
 0.190 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm24hrs; ISO 294
 0.0090 - 0.010 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm24hrs; ASTM D955
 0.010 - 0.012 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 41.0 MPaISO 527
 42.0 MPaASTM D638
Tensile Strength, Yield 48.0 MPaASTM D638
 49.0 MPaISO 527
Elongation at Break 35.1 %ASTM D638
 41.2 %ISO 527
Elongation at Yield 5.6 %ASTM D638
 5.8 %ISO 527
Tensile Modulus 2000 MPa1 mm/min; ISO 527
 2230 MPa50 mm/min; ASTM D638
Flexural Strength 75.0 MPaASTM D790
 75.0 MPaISO 178
Flexural Modulus 1840 MPaISO 178
 1890 MPaASTM D790
Izod Impact Notched 283 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 25.0 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
Dart Drop, Total Energy 28.0 Jpeak; ASTM D3763
Impact Test 61.0 JMultiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.10ASTM D3702 Modified: Manual
Coefficient of Friction, Static 0.26ASTM D3702 Modified: Manual
K (wear) Factor 42.0 x 10-10 in³-min/ft-lb-hrWasher; ASTM D3702 Modified: Manual
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 67.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 71.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 128 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80750 / 288697

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.