MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Celanex® 7416 PBT, 35% Glass Fiber/Mineral Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Product Description: Celanex 7416 is a 35% glass/mineral reinforced, non exuding, flame retarded PBT which has an excellent balance of mechanical properties and processability. Celanex 7416 is well suited for electrical applications where warp resistance or very flat surfaces are required.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Filler/Reinforcement: Glass Fiber/Mineral

Additive: Flame Retardant

Features: Flame Retardant; Low Warpage

Forms: Pellets

Processing Method: Injection Molding

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.77 g/ccISO 1183
Water Absorption 0.15 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62
Maximum Moisture Content 0.020
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 13800 psiISO 527-2/5
Elongation at Break 1.8 %ISO 527-2/5
Tensile Modulus 1.52e+6 psiISO 527-1
Charpy Impact Unnotched 12.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eU
 12.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eU
Charpy Impact, Notched 2.40 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 2.40 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Strength 810 V/milIEC 60243-1
Dissipation Factor 0.0030
@Frequency 50 Hz
IEC 60250
 0.015
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 275 V50 drops; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 437 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 401 °FUnannealed; ISO 75-2/A
Glass Transition Temp, Tg 140 °FISO 11357-2
Flammability, UL94 V-0
@Thickness 0.787 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 122 °FHopper
 482 - 500 °FHot Runner
Feed Temperature 446 - 464 °FInjection
Rear Barrel Temperature 482 - 500 °F
Middle Barrel Temperature 482 - 500 °F
Front Barrel Temperature 491 - 509 °F
Nozzle Temperature 500 - 518 °F
Zone 4 491 - 509 °FInjection
Melt Temperature 500 - 518 °F
Mold Temperature 167 - 212 °F
Drying Temperature 248 - 284 °F
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6203 / 310896

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.