MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL™ Resin PVX0901 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ PVX0901 resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This high flow, injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V1 at 1.2mm. NORYL PVX0901 resin exhibits good dimensional stabilty, low moisture absorption, low speific gravity and is an excellent candidate for internal printer components.

Features: Hydrolytic Stability,Low Creep Sensitivity,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,High Flow,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccASTM D792
Density 1.10 g/cc0.0397 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.0400 %0.0400 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.24 %0.24 %ISO 62-1
Viscosity 52 cP
@Load 5.00 kg,
Temperature 280 °C
52 cP
@Load 11.0 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 280 °C
50 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 44.0 MPa6380 psi50 mm/min; ISO 527
 45.0 MPa6530 psi50 mm/min; ASTM D638
Tensile Strength, Yield 59.0 MPa8560 psi50 mm/min; ISO 527
 60.0 MPa8700 psi50 mm/min; ASTM D638
Elongation at Break 6.6 %6.6 %50 mm/min; ASTM D638
 8.8 %8.8 %50 mm/min; ISO 527
Elongation at Yield 3.3 %3.3 %50 mm/min; ASTM D638
 3.3 %3.3 %50 mm/min; ISO 527
Tensile Modulus 2.44 GPa354 ksi1 mm/min; ISO 527
 2.50 GPa363 ksi5 mm/min; ASTM D638
Flexural Strength 86.0 MPa12500 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 95.0 MPa13800 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.30 GPa334 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.45 GPa355 ksi2 mm/min; ISO 178
Izod Impact Notched 175 J129 ft-lbASTM D256
 80.0 J
@Temperature -30.0 °C
59.0 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 37.0 J27.3 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  74.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 75.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
41.7 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  78.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
43.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
45.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 89.0 °C192 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 92.0 °C
@Thickness 3.20 mm
198 °F
@Thickness 0.126 in
unannealed; ASTM D648
 92.0 °C
@Thickness 6.40 mm
198 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 109 °C228 °FRate B/120; ISO 306
 116 °C241 °FRate B/50; ASTM D1525
 116 °C241 °FRate B/50; ISO 306
UL RTI, Electrical 65.0 °C149 °FUL 746B
UL RTI, Mechanical with Impact 65.0 °C149 °FUL 746B
UL RTI, Mechanical without Impact 65.0 °C149 °FUL 746B
Flammability, UL94 V-1
@Thickness >=1.20 mm
V-1
@Thickness >=0.0472 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 250 - 275 °C482 - 527 °F
Zone 2 225 - 270 °C437 - 518 °F
Zone 3 240 - 275 °C464 - 527 °F
Melt Temperature 250 - 275 °C482 - 527 °FInjection Molding
Mold Temperature 55.0 - 75.0 °C131 - 167 °F
Drying Temperature 75.0 - 80.0 °C167 - 176 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 30 - 70 %30 - 70 %
Vent Depth 0.00380 - 0.00510 cm0.00150 - 0.00201 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82425 / 290372

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.