MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
ThyssenKrupp XABO® 460 Structural Steel
Categories: Metal; Ferrous Metal; Carbon Steel; Low Carbon Steel

Material Notes: This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-bar impact test.

Application: These steels are applied in welded constructions such as supporting structures, vessels etc., where a secured prevention against cold cracking in the welded joints is required. Due to the low carbon equivalent, these steels are highly resistant against cold cracking.

Information Provided by Thyssen Krupp

Key Words: S460M; EN 1.8827
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 530 - 720 MPa
Tensile Strength, Yield >= 420 MPa50
 >= 440 MPa35
 >= 460 MPa
@Thickness 35.0 mm
Elongation at Break >= 17 %
Modulus of Elasticity 213 GPa
Charpy Impact 21.0 J
@Temperature -20.0 °C
Transverse
 40.0 J
@Temperature -20.0 °C
Longitudinal
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.000030 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 0.450 J/g-°C
Thermal Conductivity 45.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.14 %
Copper, Cu <= 0.30 %
Iron, Fe >= 96.4 %As Balance
Manganese, Mn <= 1.7 %
Nickel, Ni <= 0.40 %
Niobium, Nb (Columbium, Cb) <= 0.050 %
Other <= 0.45 %Carbon Equivalent
Phosphorus, P <= 0.025 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.015 %
 
Descriptive Properties
Magnetic Propertiesmagnetizable
Thermal diffusivity (cm²/s)0.13

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ThyssenKrupp PAS 460 Structural Steel for Cold Forming
ThyssenKrupp XABO® 460 T Structural Steel
ASTM A284 Steel, grade C
Evonik TEGO® Flow ZFS 460
ThyssenKrupp XABO® 500 Structural Steel

NTHYSS011 / 90331

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.