MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

MAS Epoxies DEEP POUR X Clear Casting Epoxy System
Categories: Polymer; Thermoset; Epoxy

Material Notes: The MAS Deep Pour X Epoxy Resin System is a 100% solids, two-component, two to one by volume room temperature curing epoxy resin system formulated for deep pour casting, encapsulating and molding applications. It can be cast three times as thick as the standard MAS Deep Pour epoxy resin system and allows users to complete projects twice as fast. The super slow gel time and minimally exothermic reaction allows Deep Pour X to be cast 3” thick in a single pour. It cures to a clear, glass like finish that resists scratching and yellowing It cures to a clear, glass-like finish that resists scratching and yellowing with an extended gel time to minimize exotherm and improve air release. Epoxy system specifically designed for up to 3” casting, Clear system is compatible with a variety of colorants if desired, Long gel time to mitigate yellowing and cracking during cure.

Information provided by MAS Epoxies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³Hardener; ASTM D1475
 1.11 g/cc0.0401 lb/in³Cured; ASTM D792
Viscosity 70 cP70 cPHardener; ASTM D2196
 300 cP300 cPInitial Mixed; ASTM D2196
 600 cP600 cPResin; ASTM D2196
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8383ASTM D2240
Tensile Strength 46.9 MPa6800 psiASTM D638
Elongation at Break 6.7 %6.7 %ASTM D638
Flexural Strength 66.2 MPa9600 psiASTM D790
Flexural Modulus 2.21 GPa321 ksiASTM D790
Compressive Strength 57.2 MPa8300 psiASTM D695
Izod Impact, Notched 0.427 J/cm0.800 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 46.1 °C115 °FPost cure; ASTM D648
 49.4 °C121 °FRoom Temp cure; ASTM D648
Shrinkage 4.7 %4.7 %ASTM D792/2196 (volumetric)
 
Processing PropertiesMetricEnglishComments
Gel Time 840 - 1320 min840 - 1320 min150g mass; ASTM D2471
 
Descriptive Properties
Mix Ratio by Volume2A : 1B
Mix Ratio by Weight100A : 43B
Volumetric Yield (in³/lb)24.9ASTM D792

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASZ907 / 265526

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.