MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Versalis Eraclene® BC 82 L High Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Eraclene BC 82 L is a high density polyethylene resin (HDPE), with antioxidants, suitable for blow molding application. It is especially recommended for the production of containers up to 20 liters. Eraclene BC 82 L combines a very good stress cracking resistance with a good rigidity and impact strength. This resin exhibits a high melt strength together with a moderate swelling. Eraclene BC 82 L is characterized by an intermediate molecular weight distribution which balances overall performances with ease of processing.

Application: Eraclene BC 82 L is used to produce, with high-speed machines, blow molded containers for household and industrial chemicals (detergents, bleaches, etc.) and cosmetics (shampoos, creams, lotions, etc.). Eraclene BC 82 L is suitable for thin wall items and can be extruded into profiles and sheets.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.950 g/cc0.0343 lb/in³ISO 1183
Environmental Stress Crack Resistance >= 150 hour>= 150 hourCompression Molded; ASTM D 1693(B)
Melt Flow  0.25 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 0.90 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.90 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 23 g/10 min
@Load 21.6 kg,
Temperature 190 °C
23 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6363Compression Molded; ISO 868 A
Tensile Strength at Break 30.0 MPa4350 psiISO 527
Tensile Strength, Yield 26.0 MPa3770 psiISO 527
Elongation at Break >= 600 %>= 600 %ISO 527
Flexural Modulus 1.10 GPa160 ksiISO 178
Izod Impact, Notched 1.80 J/cm3.37 ft-lb/inCompression Molded; ASTM D 256
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °FManufacturer method
Vicat Softening Point 123 °C
@Load 1.00 kg
253 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -60.0 °C<= -76.0 °FASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9838 / 265580

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.