LNP LUBRICOMP DBL349E compound is based on Polycarbonate (PC) resin containing 20% glass bead and 15% PTFE. Added features of this grade include: Wear Resistant, Flame Retardant Features: Good dimensional stability,Flame Retardant,Wear resistant Information provided by SABIC |