MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI PEXIDAN® SX505:CM493 & SX505:CM497 Moisture-curable EPDM for Low and Medium Voltage Cable Insulation
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: PEXIDAN® SX505:CM493 and SX505:CM497 is a silane crosslinkable rubber compound, curable when exposed to moist conditions. The compound can be processed on largely standard thermoplastic extrusion equipment with good extrusion properties at high output rates. The graft component SX505 is mixed with a crosslinking catalyst masterbatch CM493 or CM497 generally in the ratio 95:5. CM497 is a lower strength catalyst masterbatch and is used on thin wall extrusion or to reduce premature crosslinking during processing. The SX505:CM493 or SX505:CM497 systems have passed type-tests for use up to and including 33 kV. PEXIDAN® SX505 is a zero-halogen material and is used as insulation in Low Smoke Zero-Halogen (LSZH) cable constructions.

Information provided by SACO AEI Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792
Deformation <= 40 %
@Load 2.00 kg,
Temperature 121 °C
UL 1277 / UL 2556
Storage Temperature <= 85.0 °F
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 1305 psiUL 1277 / UL 2556
 1148 psi
@Temperature 135 °C,
Time 605000 sec
after thermal ageing; UL 1277 / UL 2556
Elongation at Break 350 %UL 1277 / UL 2556
 <= 40 %
@Temperature 250 °C,
Time 900 sec
Hot, 20 N/cm2 load; UL 1277 / UL 2556
 243 %
@Temperature 135 °C,
Time 605000 sec
after thermal ageing; UL 1277 / UL 2556
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cmASTM D6095
Dielectric Constant 2.29IEC 60250
Dissipation Factor 0.00016IEC 60250
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CScrew
Zone 1 130 °C
Zone 2 150 °C
Zone 3 180 °C
Die Temperature 200 °C
Head Temperature 190 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO007 / 249374

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.