MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Hapco SYMPOXY 1873 Epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: SYMPOXY 1873 is a two-component, room temperature curing epoxy system with a convenient 1:1 mix ratio by volume.

Information provided by Hapco, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 g/ccASTM D-4669
Water Absorption 0.030 %
@Time 86400 sec
ASTM D-570
Viscosity 3450 cPASTM D-4878
Linear Mold Shrinkage 0.00060 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65 - 75ASTM D-2240
Tensile Strength 7600 psiASTM D-638
Elongation at Break 9.6 %ASTM D-638
Izod Impact, Notched 0.980 ft-lb/inASTM D-256
Izod Impact, Unnotched 0.980 ft-lb/inASTM D-256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D-270
Dielectric Constant 3.61to 10E6 cps; ASTM D-150
Dielectric Strength 375 V/milASTM D-149
Dissipation Factor 0.030to 10E6 cps; ASTM D-150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.0 µm/m-°CASTM E-831
Thermal Conductivity 5.60 BTU-in/hr-ft²-°FASTM D-5930
Heat Distortion Temperature 60.0 °CASTM D-695
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 - 48.0 hour
@Thickness 3.17 mm
Demold
Gel Time 300 min
@Load 0.200 kg
ASTM D-2971
 
Descriptive Properties
Color (cured)Black
Mix Ratio100:100Volume
 80:100Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHAPCO170 / 317229

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.