MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Envalior ForTii® U12S PPA-I PA4T High Temperature Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: ForTii® is a high temperature polyamide for applications in the electronics, lighting, automotive, white goods, industrial and aerospace industries.

ForTii® Ace U12S is E-friendly HB and has excellent ductility and toughness and is suitable for over-molding due to its high melting temperature. Up to 120°C dry as molded or up 60°C conditioned this grade has good stiffness retention. U12S is suitable for longer term use up to 130°C. Features: Unreinforced. Processing: Injection molding.

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccDry; ISO 1183
Moisture Absorption 2.30 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cmDry; ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cmDry; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 18.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 20.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 25.0 MPa
@Temperature 140 °C
ISO 527-1/-2
 30.0 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 40.0 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 60.0 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 75.0 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
Tensile Strength, Yield 60.0 MPaCond; ISO 527-1/-2
 75.0 MPaDry; ISO 527-1/-2
 20.0 MPa
@Temperature 180 °C
ISO 527-1/-2
 21.0 MPa
@Temperature 160 °C
ISO 527-1/-2
 31.0 MPa
@Temperature 120 °C
ISO 527-1/-2
Elongation at Break 13 %
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 19 %
@Temperature 100 °C
Dry; ISO 527-1/-2
 20 %
@Temperature 23.0 °C
Cond; ISO 527-1/-2
 50 %
@Temperature 120 °C
Dry; ISO 527-1/-2
 90 %
@Temperature 180 °C
ISO 527-1/-2
 100 %
@Temperature 140 °C
ISO 527-1/-2
 100 %
@Temperature 160 °C
ISO 527-1/-2
Tensile Modulus 400 MPa
@Temperature 180 °C
ISO 527-1/-2
 410 MPa
@Temperature 160 °C
ISO 527-1/-2
 500 MPa
@Temperature 140 °C
ISO 527-1/-2
 800 MPa
@Temperature 120 °C
Dry; ISO 527-1/-2
 1700 MPa
@Temperature 100 °C
Dry; ISO 527-1/-2
 2800 MPa
@Temperature 23.0 °C
Dry; ISO 527-1/-2
 2900 MPa
@Temperature 23.0 °C
Cond; ISO 527-1/-2
Flexural Strength 110 MPaDry; ISO 178
Flexural Modulus 2500 MPaDry; ISO 178
Charpy Impact Unnotched 135 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 175 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 185 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 12.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 15.0 kJ/m²
@Temperature 23.0 °C
Cond; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmDry; IEC 60093
 >= 1.00e+13 ohm-cmCond; IEC 60093
Dielectric Strength 33.0 kV/mmCond; IEC 60243-1
 35.0 kV/mmDry; IEC 60243-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear 78.0 µm/m-°CDry; ISO 11359-1/-2
CTE, linear, Parallel to Flow 50.0 µm/m-°CDry; ISO 11359-1/-2
Melting Point 325 °C10°C/min. Dry; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 110 °CDry; ISO 75-1/-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSM7936 / 291372

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.