MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC NORYL GTX™ Resin GTX964W Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 964W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA) that exhibits very high impact resistance and high flow. This injection moldable grade was designed for large parts, such as automotive body panels, thin wall applications, and structural members for energy absorption.

Features: Chemical Resistance,Low Creep Sensitivity,Thin Wall,Low Warpage,High Impact Resistance,High Flow,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Moisture Absorption 0.0700 %0.0700 %Injection Molding
Moisture Absorption at Equilibrium 1.19 %1.19 %23°C/50% RH; ASTM D570
Water Absorption at Saturation 3.5 %3.5 %ASTM D570
Viscosity 7.0 cP
@Load 2.16 kg,
Temperature 280 °C
7.0 cP
@Load 4.76 lb,
Temperature 536 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.015 cm/cm0.015 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.013 cm/cm0.013 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527
Tensile Strength, Yield 44.0 MPa6380 psi50 mm/min; ASTM D638
 50.0 MPa7250 psi50 mm/min; ISO 527
Elongation at Break 50 %50 %50 mm/min; ISO 527
 56 %56 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %4.0 %50 mm/min; ISO 527
Flexural Strength 70.0 MPa10200 psiyield, 2 mm/min; ISO 178
 73.0 MPa10600 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 1.80 GPa261 ksi2 mm/min; ISO 178
 1.83 GPa265 ksi2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 528 J389 ft-lbASTM D256
Izod Impact, Notched (ISO) 50.0 kJ/m²23.8 ft-lb/in²80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 41.0 J30.2 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.230 W/m-K1.60 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
 185 °C
@Thickness 6.40 mm
365 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 175 °C347 °FRate B/50; ISO 306
 180 °C356 °FRate B/120; ISO 306
 240 °C464 °FRate A/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 295 - 315 °C563 - 599 °F
Zone 2 280 - 315 °C536 - 599 °F
Zone 3 290 - 315 °C554 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 75.0 - 120 °C167 - 248 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82186 / 290133

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.