MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC FLEX NORYL™ Resin WCV063 Polyphenylene Ether + TPE (PPE+TPE) (Americas)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyphenylene Ether/PPO

Material Notes: FLEX NORYL™ WCV063 resin is a flexible, non-reinforced extrusion grade of Polyphenylene Ether (PPE) + Thermoplastic Elastomer (TPE) with a Shore D Hardness rating of 63. FLEX NORYL WCV063 resin was developed for evaluation in automotive wire + cable applications requiring ISO6722 Class A or B. It exhibits ultra-thin wall capability, good scratch abrasion and pinch resistance, high dimensional stability, low shrinkage and warpage, very low water absorption, chemical resistance, and good dielectric strength. Processing is typically conducted on standard extrusion equipment, and UL 1581 testing is conducted on 2.0mm wire with 0.12mm X 20 stranded copper conductor.

Features: Flexible,Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,Good Processability,Ductile

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccASTM D792
Moisture Absorption 0.0200 %Wire Coating Extrusion
Melt Flow 33 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6310s reading; ASTM D2240
Tensile Strength at Break 25.0 MPa50 mm/min; ISO 527
 28.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 25.0 MPaISO 527
 28.0 MPa50 mm/min; ASTM D638
Elongation at Break 50 %50 mm/min; ISO 527
 90 %50 mm/min; ASTM D638
Elongation at Yield 20 %50 mm/min; ISO 527
Tensile Modulus 690 MPa1 mm/min; ISO 527
 840 MPa50 mm/min; ASTM D638
Flexural Modulus 720 MPa1.3 mm/min, 50 mm span; ASTM D790
 790 MPaISO 178
Izod Impact Notched 560 JASTM D256
 170 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 37.0 kJ/m²80*10*4; ISO 180/1A
 14.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.47
@Frequency 1e+9 Hz
ASTM D150
Dissipation Factor 0.0032
@Frequency 1e+9 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 82.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 66.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 56.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 15.0 - 30.0 °CWater Bath Temperature
 280 - 300 °CNeck Temperature
Feed Temperature 200 - 260 °C
Middle Barrel Temperature 270 - 300 °C
Die Temperature 280 - 300 °CWire Coating Extrusion
Melt Temperature 280 - 300 °CWire Coating Extrusion
Head Temperature 280 - 300 °CCross-head Temperature
 280 - 300 °C
Wire Preheat Temperature 100 - 150 °C
Drying Temperature 80.0 - 100 °CWire Coating Extrusion
Dry Time 4.00 - 6.00 hourWire Coating Extrusion
 8.00 hourCumulative; Wire Coating Extrusion
Screw Speed 5.0 - 60 rpm
 
Descriptive Properties
Compression Ratio2:1-3:1
Cooling Water Air Gap100-1000 mm
Extruder Length/Diameter Ratio (L/D)>24:1
Screen Pack60/200/60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82105 / 290052

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.