With outstanding mechanical behavior to a temperature of +210 °C, PEI EC is the solution for electrically conductive applications in relatively high temperature ranges. In addition, this material is extremely dimensionally stable (low thermal linear expansion and moisture absorption) and is highly valued for transportation systems in the electrical/electronic and semi-conductor industries.Information provided by Angst + Pfister |