40% glass fiber, general purpose, natural color Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at elevated temperatures. Markets/Uses: Automotive / Automotive E/E / Motor Brush Holders; Automotive / Automotive E/E / Solenoids Applications: Automotive Applications Features: Chemical Resistant; Good Electrical Properties Information provided by Solvay Specialty Polymers. |