MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Momentive Performance Materials SnapSil® TN3005 Low Volatile Siloxane, Silicone Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: SnapSil TN3005 is a one-component, low volatile siloxane, silicone adhesive sealant that cures at room temperature upon exposure to atmospheric moisture, and exhibits Primerless adhesion to many substrates.

Features: Fast tack-free time, Low volatility, Non-corrosive to most metals, Primerless adhesion to many substrates, Low odor cure: releases an alcohol vapor during cure, Flame retardant

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³Cured
 
Chemical PropertiesMetricEnglishComments
Ionic Impurities - Na (Sodium) <= 2.0 ppm<= 2.0 ppmCured
Ionic Impurities - K (Potassium) <= 2.0 ppm<= 2.0 ppmCured
Ionic Impurities - Cl (Chloride) <= 2.0 ppm<= 2.0 ppmCured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2222
Tensile Strength 1.80 MPa261 psi
Elongation at Break 330 %330 %
Adhesive Bond Strength 1.20 MPa174 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cmCured
Dielectric Constant 2.7
@Frequency 60 Hz
2.7
@Frequency 60 Hz
Cured
Dielectric Strength 26.0 kV/mm660 kV/inCured
Dissipation Factor 0.0020
@Frequency 60 Hz
0.0020
@Frequency 60 Hz
Cured
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Processing Temperature 23.0 °C
@Time 259000 sec
73.4 °F
@Time 72.0 hour
Cure as Tested at 50% RH
Cure Time  720 min
@Temperature 23.0 °C
12.0 hour
@Temperature 73.4 °F
1.9mm cure depth. 50% RH
 720 min
@Temperature 10.0 °C
12.0 hour
@Temperature 50.0 °F
1mm cure depth. 30% RH
 720 min
@Temperature 30.0 °C
12.0 hour
@Temperature 86.0 °F
2.7mm cure depth. 60% RH
 2880 min
@Temperature 23.0 °C
48.0 hour
@Temperature 73.4 °F
3.9mm cure depth. 50% RH
 2880 min
@Temperature 30.0 °C
48.0 hour
@Temperature 86.0 °F
4.5mm cure depth. 60% RH
 2880 min
@Temperature 10.0 °C
48.0 hour
@Temperature 50.0 °F
1.5mm cure depth. 30% RH
 4320 min
@Temperature 23.0 °C
72.0 hour
@Temperature 73.4 °F
4.8mm cure depth. 50% RH
 4320 min
@Temperature 30.0 °C
72.0 hour
@Temperature 86.0 °F
5.5mm cure depth. 60% RH
 4320 min
@Temperature 10.0 °C
72.0 hour
@Temperature 50.0 °F
1.9mm cure depth. 30% RH
Tack-Free Time 7.00 min
@Temperature 22.8 °C
0.117 hour
@Temperature 73.0 °F
50% RH
 
Descriptive Properties
Adhesion PerformanceAdhesive failurePolyethylene
 Adhesive failurePolytetraflucroethylene
 Good (cohesive failure)ABS
 Good (cohesive failure)Acrylic Resin
 Good (cohesive failure)Aluminum
 Good (cohesive failure)Copper
 Good (cohesive failure)Epoxy Resin
 Good (cohesive failure)Glass
 Good (cohesive failure)Nylon
 Good (cohesive failure)PBT
 Good (cohesive failure)PET
 Good (cohesive failure)Phenolic Resin
 Good (cohesive failure)Polycarbonate
 Good (cohesive failure)PPO
 Good (cohesive failure)PPS
 Good (cohesive failure)PVC
 Good (cohesive failure)Stainless Steel
 Good (cohesive failure)Steel
AppearanceElastic rubberCured
 Non-flamable pasteUncured
ColorClear, white, blackCured
 Clear, white, blackUncured
Volatile Siloxane (%wt)0.01Cured. (D3-D10)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9902 / 265711

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.