19-101-000-000 Description: 15% glass fiber reinforced nylon 6. Features: - Natural color
- Good stiffness
- High toughness
- Low mold shrinkage
- Electrically insulating
Applications: - Electronics
- Appliances
- Automotive
Special Instructions: Minimize back pressure to maintain glass fiber integrity.Information provided by Orion Performance Compounds, Inc. |