MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound DD0009P Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DD0009P compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, Exceptional Processing, Flame Retardant.

Features: Flame Retardant,Exceptional Processing,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.130 %0.130 %23°C/50% RH/24 hrs; ASTM D570
 0.230 %0.230 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0078 cm/cm0.0078 in/in24hrs; ISO 294
 0.0080 cm/cm0.0080 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in24hrs; ASTM D955
 0.0080 cm/cm0.0080 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 53.0 MPa7690 psiISO 527
 54.0 MPa7830 psiASTM D638
Tensile Strength, Yield 59.0 MPa8560 psiISO 527
 64.0 MPa9280 psiASTM D638
Elongation at Break 9.5 %9.5 %ISO 527
 10 %10 %ASTM D638
Elongation at Yield 4.4 %4.4 %ISO 527
 4.8 %4.8 %ASTM D638
Tensile Modulus 2.62 GPa380 ksi50 mm/min; ASTM D638
 2.80 GPa406 ksi1 mm/min; ISO 527
Flexural Strength 102 MPa14800 psiASTM D790
 102 MPa14800 psiISO 178
Flexural Modulus 2.82 GPa409 ksiASTM D790
 3.00 GPa435 ksiISO 178
Izod Impact Notched 114 J84.1 ft-lbASTM D256
Izod Impact, Unnotched 20.93 J/cm39.21 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 134 kJ/m²63.8 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 12.0 J8.85 ft-lbpeak; ASTM D3763
Impact Test 35.0 J25.8 ft-lbMultiaxial Impact; ISO 6603
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
@Thickness 3.20 mm
284 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 130 °C
@Thickness 3.20 mm
266 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=1.50 mm
V-1
@Thickness >=0.0591 in
UL 94
 V-0
@Thickness >=3.00 mm
V-0
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 290 °C509 - 554 °F
Zone 2 260 - 280 °C500 - 536 °F
Zone 3 270 - 295 °C518 - 563 °F
Melt Temperature 270 - 295 °C518 - 563 °FInjection Molding
Mold Temperature 70.0 - 95.0 °C158 - 203 °F
Drying Temperature 120 °C248 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 48.0 hour48.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81188 / 289135

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.