MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Nouryon Trigonox 23-W50 Polymer tert-Butyl peroxyneodecanoate
Categories: Other Engineering Material

Material Notes: Initiator (50% emulsion in water and methol) for suspension (co)polymerization of vinyl chloride and vinylidine chloride.

CAS number: 26748-41-4

EINECS/ELINCS No: 247-955 -1

Applications: Polymerization of vinyl chloride: Trigonox 23-W50 has an activity in between peroxydicarbonates and tert-Butyl peroxypivalate (Trigonox 25). Trigonox 23-W50 can be applied as an initiator for the suspension polymerization of vinyl chloride in the temperature range 50-65°C. The obtained polymer has a good thermal stability.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Half-life  0.100
@Temperature 84.0 °C
0.100
@Temperature 183 °F
[hr]
 1.00
@Temperature 64.0 °C
1.00
@Temperature 147 °F
[hr]
 10.0
@Temperature 46.0 °C
10.0
@Temperature 115 °F
[hr]
Viscosity 100 - 2000 cP
@Temperature -10.0 °C
100 - 2000 cP
@Temperature 14.0 °F
Molecular Weight 244.4 g/mol244.4 g/mol
Storage Temperature -25.0 - -10.0 °C-13.0 - 14.0 °F
 
Thermal PropertiesMetricEnglishComments
Decomposition Temperature 20.0 °C68.0 °FSelf-Accelerating Decomposition Temperature
 
Processing PropertiesMetricEnglishComments
Shelf Life 3.00 Month3.00 Month
 
Descriptive Properties
AppearanceWhite to off-white emulsion
Assay49.0-51.0 %
Content (%)6.55Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOURY1068 / 286591

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.