OKULEN® 1000-Reg (PE-UHMW) Ultra high molecular weight low pressure polyethylene with regenerated (recycled) materials. Properties: UV stabilized Color: UV- black FN9100/similar RAL9005 Range of applications: Mechanical engineering; Outdoor applications Information provided by Okulen |