MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco Delo® 400 Multigrade, SAE 15W-40
Categories: Fluid; Lubricant

Material Notes: Features:

Chevron Delo 400 Multigrade heavy duty motor oil is a super premium quality "universal" engine oil which exceeds industry and engine manufacturers performance requirements. It is formulated utilizing the most advanced additive technology available to provide outstanding engine protection under both pre- and post-1998 EPA exhaust particulate emissions standards for on highway diesel trucks, using both high and low sulfur diesel fuels.

Chevron Delo 400 Multigrade is formulated with ISOSYN™ base stocks, which rival synthetics in critical engine tests and an optimal blend of the latest technology in dispersant, detergent, oxidation inhibition, antiwear, corrosion inhibition, viscosity improver, and defoaming additives.

Product Applications

  • Mixed fleets pf European, North American and/or Japanese diesel engines (high-speed, four-stroke, turbocharged or naturally aspirated)
  • Commercial road transport, including vehicles with electronically-controlled engines and those designed to meet Euro 3 emissions standards
  • Commercial road transport, including electronic controlled engines and those designed to meet Euro 3 emissions standards
  • Stop-and-go vehicles in high soot loading service such as buses and waste collection trucks
  • Off-highway vehicles and plant machinery
  • Tractors and farm machinery
  • Power generation sets
  • Mobile hydraulic systems (where oil type and viscosity are appropriate)

Key Words: CPS Number: 235101; MSDS Number: 6711
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 29.6 °29.6 °
Viscosity 6400 cP
@Temperature -20.0 °C
6400 cP
@Temperature -4.00 °F
Cold Crank
Viscosity Measurement 134134Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 116 cSt116 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 15.6 cSt15.6 cStASTM D445
Ash 1.35 %1.35 %Sulfated Ash wt%
 
Chemical PropertiesMetricEnglishComments
Total Base Number 11.311.3ASTM D2896
 
Thermal PropertiesMetricEnglishComments
Pour Point -39.0 °C-38.2 °FASTM D97
Flash Point 230 °C446 °FASTM D92
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 0.138 %0.138 %
Zinc, Zn 0.151 %0.151 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow 1500 Antifoam
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Dow 1400 Antifoam
Dow 1410 ANTIFOAM
Sinotek Materials 3rd Class Carbon Rod for Dry Battery

WCHEV006 / 74621

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.