MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC XYLEX X7507 PC+Polyester (Asia Pacific)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP

Material Notes: F-1 weathering certified in natural color, specially designed for Pool & Spa applications. Currently available in natural color only.

Information provided by SABIC Innovative Plastics for Asia Pacific.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D 792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.120 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.32 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 265 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 8.0 g/10 min
@Load 2.16 kg,
Temperature 265 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 59.0 MPa50 mm/min; ISO 527
 65.0 MPaType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 61.0 MPaType I, 50 mm/min; ASTM D 638
 62.0 MPa50 mm/min; ISO 527
Elongation at Break 110 %50 mm/min; ISO 527
 130 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 5.4 %50 mm/min; ISO 527
 6.0 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2300 MPa5 mm/min; ASTM D 638
 2660 MPa1 mm/min; ISO 527
Flexural Yield Strength 92.0 MPa2 mm/min; ISO 178
 96.0 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2180 MPa2 mm/min; ISO 178
 2320 MPa1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 200 J/m
@Temperature -30.0 °C
ASTM D 256
 990 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 6.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 9.00 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 20.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 79.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
Deflection Temperature at 1.8 MPa (264 psi) 105 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 104 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 125 °CRate B/50; ASTM D 1525
 125 °CRate B/50; ISO 306
 127 °CRate B/120; ISO 306
 
Optical PropertiesOriginal ValueComments
Haze 1.6 %
@Thickness 2.54 mm
ASTM D 1003
Transmission, Visible >= 85 %ASTM D 1003

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI48710 / 189795

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.