System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Petropol Nypol® A3 G10 UV PRTA011 NR436 Nylon 66, 10% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
;
Nylon 66, 10% Glass Fiber Filled
Material Notes:
Product Description: 10% Glass Fiber, UV Stabilized, Polyamide 6.6
Resin ID (ISO 1043): PA66 GF10
Processing: Injection Molding
Color: Black
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.21
g/cc
ASTM D792
Water Absorption
2.22 %
Humidity Absorption; ASTM D570
7.1 %
ASTM D570
Maximum Moisture Content
0.20
Linear Mold Shrinkage
0.0060
cm/cm
ASTM D955
Deformation
1.1 %
@Pressure 27.6 MPa,
Temperature 50.0 °C
ASTM D621
Ash
8.0 - 12 %
ASTM D2584
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
118
MPa
ASTM D638
Tensile Strength
120
MPa
ASTM D638
Elongation at Break
3.0 %
ASTM D638
Tensile Modulus
5500
MPa
ASTM D638
Flexural Strength
190
MPa
ASTM D790
Flexural Modulus
5300
MPa
ASTM D790
Shear Strength
75.0
MPa
ASTM D732
Izod Impact, Notched
48.0
J/m
ASTM D256
Izod Impact, Notched (ISO)
0.00214
ft-lb/in²
ASTM D256
Izod Impact, Unnotched (ISO)
0.0190
ft-lb/in²
ASTM D256
Charpy Impact Unnotched
32.0
J/cm²
ASTM D256
Charpy Impact, Notched
4.50
J/cm²
ASTM D256
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+16
ohm-cm
IEC 60093
Thermal Properties
Original Value
Comments
Melting Point
250
-
265
°C
ASTM D2217
Deflection Temperature at 1.8 MPa (264 psi)
230
°C
ASTM D648
Flammability, UL94
HB
@Thickness 2.00 mm
Processing Properties
Original Value
Comments
Processing Temperature
260
-
280
°C
Molding
Mold Temperature
65.0
-
120
°C
Drying Temperature
80.0
°C
Dry Time
4.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPETROPOL105 / 313013
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.