MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC SABIC® PP G3220A PP (Americas)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: SABIC® PPcompound G3220A is a 20% short glass fiber reinforced Polypropylene for under-the-hood and structural applications. The base material is a PP homopolymer. The glass fibres are chemically coupled to the PP matrix. This material has been designed to combine a good performance profile with fast processing. SABIC® PPcompound G3220A is a designated automotive grade. IMDS ID: 209767996

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Density 1.04 g/ccISO 1183
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa50 mm/min, 1A; ISO 527
 87.0 MPa50 mm/min; ASTM D638
Elongation at Break 3.3 %50 mm/min; ISO 527
 3.3 %50 mm/min; ASTM D638
Tensile Modulus 4900 MPa1mm/min; ISO 527
 5380 MPa50 mm/min; ASTM D638
Flexural Modulus 4210 MPa1.3 mm/min, 50 mm span; ASTM D790
 4500 MPa2 mm/min, 64mm span; ISO 178
Izod Impact, Notched 9.00 J/m80*10*4mm, Cut; ISO 180/1A
 75.0 J/m63.5*12.7*3.2mm, Cut; ASTM D256
Izod Impact, Unnotched 601 J/m63.5*12.7*3.2mm, Cut; ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 10.0 kJ/m²80*10*4mm, Cut; ISO 179/1eA
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4mm, Cut; ISO 179/1eA
Dart Drop, Total Energy 7.00 Jpeak, 23°C @ 2.2 m/s; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
CTE, linear, Transverse to Flow 163 µm/m-°C
@Temperature -30.0 - 100 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 161 °C80*10*4mm, Cut; ISO 75-1&2
 160 °C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 150 °C80*10*4mm, Cut; ISO 75-1&2
 151 °C
@Thickness 3.20 mm
ASTM D648
Vicat Softening Point 163 °C10N, 50°C/hr; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 210 - 270 °CInjection Molding
Zone 1 190 - 230 °C
Zone 2 200 - 250 °C
Zone 3 210 - 270 °C
Melt Temperature 210 - 270 °C
Mold Temperature 15.0 - 60.0 °C
Drying Temperature 80.0 - 100 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Back Pressure 1.00 - 1.50 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI11525 / 244992

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.