MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound D451 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP THERMOCOMP D451 compound is based on Polycarbonate (PC) resin containing 40% glass fiber. Added features of this grade include: High Modulus, Low Warpage, Good Ductility, Non-Brominated & Non-Chlorinated Flame Retardant.

Features: High Stiffness,Enhanced Ductility,Flame Retardant,Non-Chlorinated,Non-Brominated,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
Viscosity  14 cP
@Load 2.16 kg,
Temperature 300 °C
14 cP
@Load 4.76 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
 42 cP
@Load 5.00 kg,
Temperature 300 °C
42 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.0010 - 0.0025 cm/cm0.0010 - 0.0025 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0010 - 0.0025 cm/cm0.0010 - 0.0025 in/in24hrs; ASTM D955
Melt Flow  17.9 g/10 min
@Load 2.16 kg,
Temperature 300 °C
17.9 g/10 min
@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
 57 g/10 min
@Load 5.00 kg,
Temperature 300 °C
57 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 143 MPa20700 psi5 mm/min; ASTM D638
Elongation at Break 2.3 %2.3 %5 mm/min; ASTM D638
Tensile Modulus 11.72 GPa1700 ksi5 mm/min; ASTM D638
Flexural Strength 186 MPa27000 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 9.75 GPa1410 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 140 J103 ft-lbASTM D256
Izod Impact, Unnotched 5.21 J/cm9.76 ft-lb/inASTM D4812
Charpy Impact Unnotched 3.30 J/cm²15.7 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²6.19 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
8.56 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow 56.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
31.3 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 114 °C
@Thickness 3.20 mm
237 °F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical 80.0 °C176 °FUL 746B
UL RTI, Mechanical with Impact 80.0 °C176 °FUL 746B
UL RTI, Mechanical without Impact 80.0 °C176 °FUL 746B
Flammability, UL94  V-1
@Thickness >=0.600 mm
V-1
@Thickness >=0.0236 in
UL 94
 V-0
@Thickness >=0.800 mm
V-0
@Thickness >=0.0315 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 285 - 305 °C545 - 581 °F
Zone 2 270 - 290 °C518 - 554 °F
Zone 3 280 - 300 °C536 - 572 °F
Melt Temperature 285 - 310 °C545 - 590 °FInjection Molding
Mold Temperature 80.0 - 110 °C176 - 230 °F
Drying Temperature 110 °C230 °FInjection Molding
Dry Time 3.00 - 6.00 hour3.00 - 6.00 hourInjection Molding
Back Pressure 0.100 - 0.300 MPa14.5 - 43.5 psi
Screw Speed 50 - 90 rpm50 - 90 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81488 / 289435

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.