MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem Naugard™ P Antioxidant
Categories: Other Engineering Material

Material Notes: Product Description: Naugard™ P phosphite is a cost effective secondary liquid phosphate antioxidant that functions as a peroxide decomposer and as a processing stabilizer. When used in conjunction with hindered phenolic and thiodipropionate antioxidants, a synergism is seen. In addition to improved antioxidant activity of these combinations, Naugard™ P phosphate also inhibits discoloration of the polymer caused by some phenolic antioxidants, Polymer applications include polyolefins, styrenics and a variety of other polymers.

Features: FDA regulated; Non-discoloring; Liquid physical form; Economical; Low volatility

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.978 g/cc
Viscosity 5200 cP
Molecular Weight 688 g/mol
 
Thermal PropertiesOriginal ValueComments
Pour Point -7.00 °F
Flash Point 430 °FTOC
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 2.0
 
Descriptive Properties
AppearanceClear viscous liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH507 / 315425

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.