MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical Goyenchem-MA Melamine Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Intro: Goyenchem-MA, melamine flame retardant, also known as Cyanuramiden, is an organic base and a trimer of cyanamide. Resin products with Melamine will release abundant nitrogen when heated, thus can be applied to flame retardant, waterproofing agent, and Formaldehyde remover…etc. Goyenchem-MA is a high-performance flame retardant developed by GYC Group and is targeted at extensive plastic, rubber, and resin industry.

Advantages:

  • Excellent flame retardant performance
  • Free of fluorine, chlorine, bromine, and other halogens
  • High decomposition temperature
  • Good compatibility and dispersity with various resin, copolymer, engineering plastics, and coatings
  • Reduce occurrence of continuous burning caused by polymer dipping
  • Goyenchem-MA is a certified item by world giant of plastic, rubber, resin, and coating manufacturers.
Applications:
  • Flame retardant plastics& coatings
  • Anti-wrinkle, anti-shrinking additive
  • Leather processing tanning agent and filler
  • Synthetic fireproof laminates adhesive, waterproof, and curing agent
  • Solvent Polyurethane leveling agent
  • Other complex FR applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 7.5 - 9.5
Ash <= 0.030 %
 
Optical PropertiesOriginal ValueComments
Haze 30 %(bolus alba) Degree
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %
 
Descriptive Properties
AppearanceWhite Powder
Color=20APHA
Composition>99.8%MELAMINE

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN071 / 266379

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.