Polypropylene homopolymer 50% glass fibers reinforced, chemically coupled, very good mechanical properties. Available: all colors, UV stabilized (L), heat stabilized (H), high heat stabilized (HT), laser printable (LP), detergent stabilized (D).Information provided by Taro Plast S.p.a. |