MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis Riblene® FM 53 F Film Grade Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Riblene FM 53 F is a LDPE, with slip and antiblocking agent, suitable for blown film extrusion. Riblene FM 53 F is characterized by optimum optical properties and rigidity. Films manufactured by Riblene FM 53 F are easily heat shrinkable.

Application: Riblene FM 53 F is recommended for automatic packaging where low gauge films having a certain rigidity and gloss are required (hygienic packaging).

Property values reported for film extruded with BUR 1:3, thickness 70 µm. Actual properties are typical and may vary depending upon operating conditions and additive package.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.933 g/cc0.0337 lb/in³ISO 1183
Thickness 18.0 - 50.0 microns0.709 - 1.97 milRecommended
 70.0 microns2.76 milAs-tested; BUR 1:3
Melt Flow 3.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 14.0 MPa2030 psiISO 527-3
Film Tensile Strength at Yield, TD 15.0 MPa2180 psiISO 527-3
Film Elongation at Break, MD 350 %350 %ISO 527-3
Film Elongation at Break, TD 600 %600 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.14>= 0.14ISO 8295
Elmendorf Tear Strength, MD 5.10 g/micron130 g/milISO 6383-2
Elmendorf Tear Strength, TD 6.60 g/micron168 g/milISO 6383-2
Dart Drop Test 80.0 g0.176 lbF50; ISO 7765-1/A
Film Tensile Strength at Break, MD 21.0 MPa3050 psiISO 527-3
Film Tensile Strength at Break, TD 20.0 MPa2900 psiISO 527-3
1% Secant Modulus, MD 300 MPa43500 psiISO 527-3
1% Secant Modulus, TD 310 MPa45000 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 118 °C244 °FManufacturer method
Vicat Softening Point 107 °C
@Load 1.00 kg
225 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D 746
 
Optical PropertiesMetricEnglishComments
Haze 7.0 %7.0 %ISO 14782
Gloss 70 %70 %45°; ASTM D 2457
 
Processing PropertiesMetricEnglishComments
Processing Temperature 150 - 170 °C302 - 338 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9820 / 265698

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.