LNP ELCRES DMX1435D is a UV stabilized standard flow Polycarbonate (PC) copolymer resin with diffusion effect and improved scratch resistance. This grade is a good candidate for consumer electronics, mobility interiors and other adjacent applications, which need lower scratch and diffusive effects performance. Features: Scratch Resistance,UV Resistant Information provided by SABIC |