MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC CYCOLOY™ FR C6600 PC+ABS (Americas)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY C6600 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable non chlorinated/brominated flame retardant grade with balanced flow, impact and hydrolytic stability. It also offers good chemical resistance and colorability in opaque colors. It has a UL94 V0@1.5mm and 5VB@2.0mm flame rating.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Water Absorption 0.11 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 21.5 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 49.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 63.0 MPa50 mm/min; ASTM D638
Elongation at Break 80 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ASTM D638
Tensile Modulus 3000 MPa50 mm/min; ASTM D638
Flexural Yield Strength 94.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2620 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 550 J/mASTM D256
Dart Drop, Total Energy 51.0 JASTM D3763
 51.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.7
@Frequency 1e+6 Hz
IEC 60250
 2.7
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
Dissipation Factor 0.0040
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 99.0 °CRate B/50; ASTM D1525
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 70.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.750 mm
UL 94
 V-0
@Thickness 1.50 mm
UL 94
 5VB
@Thickness 2.00 mm
UL 94
Glow Wire Test 775 °C
@Thickness 1.00 mm
IEC 60695-2-13
 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 275 °CInjection Molding
Zone 1 220 - 255 °C
Zone 2 220 - 275 °C
Zone 3 245 - 275 °C
Melt Temperature 245 - 275 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 80.0 - 90.0 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 80 %
Vent Depth 0.00380 - 0.00760 cm
Screw Speed 40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10785 / 244252

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.