MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SACO AEI THERMODAN® HF TP0842N Low Smoke Zero Halogen Jacket Compound For Power-Limited Circuit Cables (Provisional)
Categories: Polymer; Thermoplastic

Material Notes: Product THERMODAN® HF TP0842N is a Low Smoke Halogen-Free, Thermoplastic Wire and Cable Compound. This compound has superior fire performance, low smoke production and contains no halogens. It is a jacket compound for cables recognized under UL 13 Power-Limited Circuit Cables; Principally for Class 2 (CL2) and Class 3 (CL3) cables. THERMODAN® HF TP0842N is natural in color and UV resistant.

Applications:

  • Thin Wall LSZH Insulation and Jackets recognized under UL 13 for CL2 and CL2X cables
Features & Benefits
  • Shown to be capable of VW-1 performance when applied at 30 mil on 14 AWG copper conductor
  • Natural compound color adaptable to a wide variety of jacket color options

Information provided by SACO AEI Polymers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.53 g/ccASTM D792
Melt Flow 2.7 g/10 min
@Load 21.6 kg,
Temperature 150 °C
ASTM D1238
Storage Temperature <= 300 °F
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break >= 1700 psiUL 2556
 >= 1445 psi
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 2556
Elongation at Break >= 140 %UL 2556
 >= 112 %
@Treatment Temp. 121 °C,
Time 605000 sec
after thermal ageing; UL 2556
Tear Strength 30.2 pliASTM D624
 
Thermal PropertiesOriginal ValueComments
Oxygen Index 43 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Processing Temperature 135 - 171 °Cbarrel
Die Temperature 179 °C
Head Temperature 177 °C
Drying Temperature 60.0 °C
@Time 14400 sec
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSACO083 / 265513

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.