MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Grupo Repol Dinalon® B1S25 G50 50% Glass Fiber Reinforced Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Mechanical properties are for dry as molded samples.

Information provided by Grupo Repol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183/A
Moisture Absorption at Equilibrium <= 0.25 %<= 0.25 %Karl-Fischer; ISO 15512/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Flexural Strength 340 MPa49300 psiISO 178
Flexural Modulus 13.0 GPa1890 ksiISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
@Temperature 23.0 °C
8.09 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.80 J/cm²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FISO 75/A
Vicat Softening Point >= 200 °C>= 392 °F50 N; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kolon KOPA® KN133G50 G/F Reinforced Nylon 6
Eurotec® Tecomid® NB40 GR50 NL PA 6 50% glass fiber reinforced
Epsan Eplamid 6 GFR 50 NC Q1F001 Polyamide 6
Envalior Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
Celanese Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced

PGRU022 / 43284

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.