Single-component Release Coat® keeps hot rubber and asphalt from sticking to corrugated containers without the use of a costly plastic bag. It is easy to use, requires no mixing, is corrugator-applied and repulpable. Release Coat® P1 HS must be combined with Catalyst P1 before applying to a substrate. This product may be applied by rod or blade coater. Usage: Release Coat® P1 HS is one part of a two part silicone release coating. A catalyzed release coat system offers superior release and in most cases FDA compliance. This system is not gluable. Applications (properties imparted): Industrial (release).Handling: Handle in accordance with good industrial hygiene and safety practice. Use personal protective equipment as required. Information provided by Michelman |