MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials PC LSG Extruded (ISO Data)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Within its portfolio of Life Science Grade Engineering Plastic Products - specifically developed for applications in the medical, pharmaceutical and biotechnology industries - Mitsubishi Chemical Advanced Materials offers LSG PC natural biocompatible engineering plastic stock shapes for machining with certified USP Class VI and ISO 10993 compliance

  • High mechanical strength
  • Good creep resistance
  • Very high impact strength, even at low temperatures
  • Stiffness retention over a wide range of temperatures
  • Very good dimensional stability (very low water absorption and low coefficient of linear thermal expansion)
  • Natural colour (clear, translucent)
  • Good electrical insulating and dielectric properties
  • Physiologically inert (suitable for food contact)
  • Economical thermal performance

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
K Factor (ISO) 60 µm/km
Coefficient of Friction, Dynamic 0.50 - 0.60
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
USP Class VI Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Unacceptable
Acids, Weak Limited
Alcohols Limited
Alkalies, Strong (pH 11-14) Unacceptable
Alkalies, Weak Limited
Chlorinated Solvents Unacceptable
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Unacceptable

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Altron™ PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet)
Overview of materials for Polycarbonate, Extruded
Applied Nanostructured Solutions PC/ABS - Carbon NanoStructure Chopped Fiber Composite
Mitsubishi Iupilon® MB 8500 PC/ABS
Overview of materials for Polycarbonate, 20% Glass Filled

P1SMU906 / 130693

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.