MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound ZX08309 Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: LNP THERMOCOMP ZX08309 compound is based on Polyphenylene Ether / Polystyrene (PPE/PS) blend containing proprietary fillers. Added features of this grade include: High Dielectric Constant and Low Loss Tangent.

Features: Dielectrics,Circuit Solution

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.66 g/cc0.0600 lb/in³ISO 1183
Viscosity 11 cP
@Load 5.00 kg,
Temperature 300 °C
11 cP
@Load 11.0 lb,
Temperature 572 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0070 cm/cm0.0070 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0065 cm/cm0.0065 in/in24hrs; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 90.0 - 100 MPa13100 - 14500 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.20 - 3.50 GPa464 - 508 ksi2 mm/min; ISO 178
Izod Impact Notched 60.0 J44.3 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.4 - 4.6
@Frequency 1.10e+9 Hz
4.4 - 4.6
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Dissipation Factor 0.0020 - 0.0040
@Frequency 1.10e+9 Hz
0.0020 - 0.0040
@Frequency 1.10e+9 Hz
ASTM ES 7-83
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 134 °C
@Thickness 3.20 mm
273 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
@Thickness 3.20 mm
252 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 290 - 295 °C554 - 563 °F
Zone 2 290 - 295 °C554 - 563 °F
Zone 3 300 - 305 °C572 - 581 °F
Melt Temperature 295 - 305 °C563 - 581 °FInjection Molding
Mold Temperature 90.0 °C194 °F
Drying Temperature 105 °C221 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 9.00 MPa1310 psi
Screw Speed 100 rpm100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81992 / 289939

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.