MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Angst+Pfister APSOplast® PC EC PC + electrically conductive surface coating
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: PC EC is a scratch-resistant polycarbonate characterized by electrically conductive surfaces (surface resistance of 103–105 O) and excellent transparency and translucency as well as high impact resistance and dielectric strength. This challenging combination of properties is always in demand for glazing material in special production areas where electrostatic charging must be avoided.

Information provided by Angst + Pfister

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN EN ISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 60.0 MPa50 mm/min; DIN EN ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; DIN EN ISO 527
Elongation at Break 70 %50 mm/min; DIN EN ISO 527
Elongation at Yield 6.0 %50 mm/min; DIN EN ISO 527
Modulus of Elasticity 2.40 GPa1 mm/min; DIN EN ISO 527
Flexural Strength 100 MPa2 mm/min; ISO 178
Charpy Impact Unnotched NBDIN EN ISO 179-1eU
Charpy Impact, Notched 11.0 kJ/m²DIN EN ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1e+05 - 1.00e+7 ohmIEC 60093
Dielectric Constant 12IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°CDIN 53752
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
Haze >= 1.0 %
Transmission, Visible 89 %
@Thickness 3.00 mm
DIN 5036 / ASTM D-1003 / ISO 13468-1/-2
 
Descriptive Properties
Colorclear transparent
Light reflectance factor8DIN 5033/5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PANGP020 / 250518

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.