MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Eastman TamiSolve® NxG
Categories: Fluid; Solvent

Material Notes: Product Description: TamiSolve® NxG is a high boiling, dipolar aprotic solvent. TamiSolve® NxG has a good solvency for a wide range of compounds and has a high chemical and thermal stability. TamiSolve® NxG has an established performance in specialty polymer coatings (wire enamels & coated cooking gear), micro-electronics manufacturing (photoresist stripper), coatings (PUD’s), paint strippers and inks, chemical synthesis and agrochemical formulations. In many applications it can be used to replace NMP or NEP (N (m)ethylpyrrolidone), as well as other solvents like dimethyl sulfoxide (DMSO) and Dipropylene Glycol Dimethyl Ether (DMM). As opposed to NMP and NEP, TamiSolve® NxG is not classified as developmental reprotoxic.

Application/Uses:

  • Agrochemical industry
  • Chemicals and Pharmaceuticals synthesis
  • Electronics industry
  • Inks
  • Paints, coatings & resins
  • Polymer manufacture (Polyamide imids & Polyimids)
  • PU Coatings & Synthetic leather

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
pH 7.657.6510% solution in water
Viscosity 4.0 cP4.0 cP
Molecular Weight 141.21 g/mol141.21 g/mol
Vapor Pressure 0.000345 bar0.258 torr
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.98 J/g-°C0.473 BTU/lb-°F
Thermal Conductivity 121 W/m-K840 BTU-in/hr-ft²-°F
Melting Point <= -75.0 °C<= -103 °FFreezing Point
Boiling Point 241 °C466 °F
Flash Point 108 °C226 °FClosed Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.46751.4675

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Water, H2O
Overview of materials for Vinyl Ester Sheet Molding Compound
Overview of materials for Brass
Diamond, Synthetic
Aluminum 6061-T6; 6061-T651

PEATM5604 / 222798

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.