MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Reynolds EZ~Spray® Plastic Sprayable Urethane Plastic Compound
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: EZ~Spray® Plastic is an improved version of our original sprayable polyurethane plastic compound. With higher impact resistance, this new spray plastic was specifically formulated to be mixed and sprayed via Smooth-On’s EZ~Spray® Jr. Spray System. EZ~Spray® Plastic is versatile and can be sprayed over a rubber mold to create “mother molds” or support shells. It can also be sprayed or meter mixed into rubber molds as a fast setting casting resin. Cured plastic is lightweight, tough and durable. EZ~Spray® Plastic has a fast gel time for vertical surface application. Material cures in about 3 hours (depending on mass). Refer to the EZ~Spray® Machine Jr. Video Manual before spraying plastic.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D-1475
Linear Mold Shrinkage 0.016 cm/cm0.016 in/inASTM D-2566
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575ASTM D-2240
Tensile Strength, Ultimate 18.3 MPa2650 psiASTM D-638
Elongation at Break 10 %10 %ASTM D-638
Tensile Modulus 0.689 GPa100 ksiASTM D-638
Flexural Strength 34.5 MPa5000 psiASTM D-790
Flexural Modulus 1.05 GPa153 ksiASTM D-790
Compressive Strength 34.5 MPa5000 psiASTM D-695
Compressive Modulus 0.310 GPa45.0 ksiASTM D-695
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 55.0 °C131 °FASTM D-648
 
Processing PropertiesMetricEnglishComments
Cure Time 180 min3.00 hourHandling Time
Pot Life 0.0330 min0.0330 minASTM D-2471
 
Descriptive Properties
ColorOff-White
Mix Ratio1A:1B pbvby volume
Mixed ViscosityVariable
Specific Volume25[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN054 / 296755

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.