OKULEN® 2000-OF 7010 is a oil filled UHMW Polymer. This material was designed for perform in conveying systems used in the food industry. Further, it helps reduce noise levels with its excellent gliding properties. This UHMW is known for its great impact strength and abrasion resistance surface quality. Properties: Good gliding properties; Water repellent; Great noise reduction; EU 1935/2004 & 10/2011 – conform; FDA – conform Color: grey FN7010; OK-Nr 7010 Range of applications: Conveyor industry, Bearings Information provided by Okulen |