MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Toyobo Fortron® FX55T1 PPS, Impact Modified
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS); Molded

Material Notes: Product Description: Forton FX55T1 is an unreinforced, impact modified PPS with high melt viscosity suitable for extrusion.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Additive: Impact Modifier

Features: Impact Modified

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.015 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 7250 psiISO 527-2/50
Tensile Strength, Yield 7980 psiISO 527-2/50
Elongation at Break 40 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 334000 psiISO 527-1
Flexural Strength 102000 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 331000 psiISO 178
Charpy Impact Unnotched NBISO 179/1eU
Charpy Impact, Notched 17.0 ft-lb/in²
@Temperature -30.0 °C
ISO 179/1eA
 29.0 ft-lb/in²
@Temperature 22.8 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 44.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 53.0 µin/in-°FISO 11359-2
Specific Heat Capacity 0.359 BTU/lb-°FASTM E1461
Melting Point 536 °FISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 212 °FUnannealed; ISO 75-2/A
Vicat Softening Point 320 °FISO 306/B50
 518 °FISO 306/A50
 
Processing PropertiesOriginal ValueComments
Processing Temperature 68.0 - 86.0 °FHopper
 599 - 608 °FHot Runner
Feed Temperature 167 - 185 °FInjection
Rear Barrel Temperature 572 - 590 °F
Middle Barrel Temperature 581 - 599 °F
Front Barrel Temperature 590 - 608 °F
Nozzle Temperature 599 - 608 °F
Zone 4 590 - 608 °FInjection
Melt Temperature 599 - 608 °F
Mold Temperature 275 - 302 °F
Drying Temperature 212 °F
Dry Time 3.00 - 4.00 hour
Back Pressure <= 508 psi
Screw Speed 50 rpm
@Thickness 55.9 mm
 75 rpm
@Thickness 40.6 mm
 120 rpm
@Thickness 24.9 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHCQ6287 / 310980

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.